Tumble finishing, also known as tumbling or rumbling, is a technique for smoothing and polishing a rough surface on relatively small parts. In the field of metalworking, a similar process called barreling, or barrel finishing, works upon the same principles.

This process is very similar to the natural processes that produce "sea glass" or "beach glass".

For tumbling of rocks as a lapidary technique, a plastic or rubber-lined barrel is loaded with a consignment of rocks, all of similar or the same hardness, some abrasive grit, and a liquid lubricant. Silicon carbide grit is commonly used, and water is a universal lubricant. The barrel is then placed upon slowly rotating rails so that it rotates. The optimal speed of rotation depends on the size of the tumbler barrel and materials involved.

A well-chosen speed for stone polishing causes the rocks within the barrel to slide past each other, with the abrasive grit between them. The result of this depends on the coarseness of the abrasive, and the duration of the tumble.

Typically, a full tumble polish from rough rock to polish takes between 3–5 weeks, and is done in a minimum of 3 steps. Initially, the rocks are smoothed with a coarse grit (such as 60-90 mesh). The idea behind the first step is to take rough rock or stone and grind it (tumble it) down into a form which is indistinguishable (in shape) from the final product. This is followed by washing and then a stage of finer grits (120-220 then 400-600 mesh), before the (optional) use of a pre-polishing compound (1200 grit), a washing cycle with detergent to remove any grit on the stones. The final step is a polishing stage using powdered polish, (such as cerium oxide or tin oxide), water, and often small plastic pellets that are designed to cushion the stones as they tumble (so as not to cause chipping) and carry the polish evenly across the stones.

The precise tumbling duration is determined by many factors, including the hardness of the rock and the degree of smoothing desired in the coarser steps. Some people will tumble stones with rough grit for two, three or even four weeks to get their desired shapes out of the stones.


...